Stretching descaler has insufficient stretching coefficient, so that the iron sheet is not fully broken and peeled, which affects the pickling effect;
Strip steel shape is poor, such as sickle bend, wave shape, etc., so that the mechanical descaling effect is poor, easy to cause partial under-washing.
The surface has a large area of point defects, generally appearing on one side, comprehensive, white after annealing, and black spots after leveling.
The annealed steel coils are bonded together to each other, which is called bonding. After the flattening, the point-like circular arc creases are point-stick; the arc-shaped creases appearing in the rolling direction are strip-shaped bonds; serious surface bonding, The flat unwinding is torn or voids become a waste roll.
| HSLA Grades | C | Mn | P | S | Cu | Mo | V | Cb | Ti |
|---|---|---|---|---|---|---|---|---|---|
| 45C1 | 0.22 | 1.35 | 0.04 | 0.04 | 0.2 | 0.06 | 0.005 | 0.005 | 0.005 |
| 45C2 | 0.15 | 1.35 | 0.04 | 0.04 | 0.2 | 0.06 | 0.005 | 0.005 | 0.005 |
| 50C1 | 0.23 | 1.35 | 0.04 | 0.04 | 0.2 | 0.06 | 0.005 | 0.005 | 0.005 |



Hot Tags: cold annealed steel coil, China, suppliers, manufacturers, factory, buy, price, pricelist, for sale, in stock, free sample, Cold Rolled Mild Steel Sheet, Cold rolled Steel Sheet, Cold Rolled Steel Strips, SPCC Cold Rolled Steel, Cold Rolled Steel Coils, SPCD Cold Rolled Steel Sheet