Chemical composition % of the ladle analysis of grade SC2
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Al(%) | Ti(%) |
| Max 0.01 | Max 0.03 | Max 0.03 | 0.02 | 0.02 | — | Max 0.20 |
| Proof strength Rp0.2 (MPa) | Tensile strength Rm (MPa) | Impact energy KV (J) | Elongation at fracture A(%) | Reduction in cross section on fracture Z(%) | As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 797 (≥) | 464 (≥) | 12 | 11 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
| Property | Density kg/dm3 | Temperature T °C/F | Specific heat J / kgK | Thermal conductivity W/mK | Electric resistance µΩ·cm | Modulus of elasticity kN/mm2 | Expansion rate |
|---|---|---|---|---|---|---|---|
| 643 (≥) | 749 (≥) | 11 | 41 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 | |
| Temp. °C/°F | Creep strain limit (10000h) (Rp1,0) N/mm2 | Creep rupture strength (10000h) (Rp1,0) N/mm2 | |||||
| 212 | 898 | 567 |
| Product type | Products | Dimension | Processes | Deliver Status |
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |