The protective gas dew point is too high or the hydrogen content is too low. The pre-washing time is insufficient before heating, residual oxygen exists in the furnace, and the residual cold rolled steel coil is annealed in an oxidizing atmosphere.
The surface of the steel strip is caused by the oil film rupturing and the steel strip is in direct contact with the work roll.
GRADE | C% max | Mn% max | P% max | S% max | Alt% min | Ti max |
SC2 | 0.06 | 0.35 | 0.025 | 0.025 | 0.015 | 0.20 |