Type 302 (18/8 chrome-nickel) Austenitic. This type differs but little from its companion Alloy Type 301. However, the slight increase in Chromium and Nickel contents in Type 302 over 301 develops marked changes in its mechanical properties and in its forming behavior. Type 302 work hardens much less rapidly than does Type 301 but with strength and toughness second only to 301 stainless steel. It possesses excellent heat and corrosion resistance and welds easily.
Chemical Composition (%) of 302 Stainless Steel Plate
| Cr | N | Mn | C | S | P | Si |
| 17-19 | 8-10 | 2.00 max | 0.15 max | 0.030 max | 0.045 max | 1.00 max |
To solution anneal, cool rapidly in air or water from about 2000° F. It is not heat treatable for hardening purposes and is slightly magnetic following cold working. We stock Type 302 in five different tempers - Soft to Full Hard inclusive.