Grade 420 is a martensitic stainless steel designation that covers both the wrought 13% chromium base metal and the matching 420-type welding consumable specified in EN ISO 14343. Its higher carbon content, compared with the 410 and 430 grades, is what gives the material its response to heat treatment: it can be hardened and tempered to deliver the combination of hardness, wear resistance and moderate corrosion resistance demanded by cutlery, valve parts, shafts and turbine components.
This article sets out the chemical composition, the mechanical properties in the annealed and in the quenched and tempered condition, the equivalent grade relationships, and the welding and heat treatment rules that govern the final properties of a grade 420 joint.
What Grade 420 Martensitic Stainless Steel Is
EN ISO 14343 covers wire electrodes, strip electrodes, wires and rods for arc welding of stainless and heat-resisting steels. Within that standard the 420 type is a martensitic stainless filler in the 13% chromium family, used to weld martensitic stainless steels such as the AISI 420 grades in services that require hardness and wear resistance. The deposited weld metal has a martensitic structure and can be hardened by heat treatment, so the properties reached in service depend on the post-weld thermal cycle as much as on the consumable itself.
Grade 420 therefore occupies a defined position in the stainless family. After hardening and tempering it is harder and stronger than grade 410, but it is less corrosion resistant than the chromium-nickel austenitic grades and less tough than the low-carbon martensitic grades. Selection should always be based on the balance of hardness, strength and corrosion resistance that the application actually needs.
Chemical Composition of the 420 Type
The table below gives the 420 type analysis specified for welding consumables. Wrought base metals in the same family are matched to this analysis so that the joint reaches the required mechanical properties after heat treatment.
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.25-0.40 |
| Silicon (Si) | ≤ 0.50 |
| Manganese (Mn) | ≤ 0.60 |
| Nickel (Ni) | ≤ 0.75 |
| Phosphorus (P) | ≤ 0.03 |
| Sulfur (S) | ≤ 0.03 |
| Chromium (Cr) | 12.0-14.0 |
| Molybdenum (Mo) | ≤ 0.75 |
| Copper (Cu) | ≤ 0.75 |
Chromium in the 12.0-14.0% range builds the passive surface film that provides atmospheric corrosion resistance, while carbon in the 0.25-0.40% range makes the martensitic transformation and the hardening response possible. Silicon, manganese and nickel are balanced to control deoxidation and to keep the weld metal within a workable hardness window, while phosphorus and sulfur are held at low levels to limit hot cracking and loss of toughness.
Mechanical Properties in the Annealed Condition
Annealed weld metal in the 13% chromium family is normally supplied in the softest and most machinable condition. Typical order-of-magnitude values are 450 MPa tensile strength, 250 MPa proof strength and 15% elongation. In this condition the structure is comparatively soft and ductile, which suits machining and forming and suits joints that will be heat treated after welding rather than used as-welded.
Because the annealed condition is defined by a specific cooling cycle, the same chemistry can produce different results if the cooling rate changes. The guaranteed values for a particular consumable are those stated on the manufacturer's data sheet for the governing edition of the standard.
Mechanical Properties After Quenching and Tempering
Hardening and tempering is the normal route to the properties for which grade 420 is selected. Quenched and tempered weld metal reaches substantially higher strength and hardness than the annealed condition, with the exact levels set by the austenitising temperature, the quenching medium and, above all, the tempering temperature. Low tempering temperatures give the highest hardness for wear applications, while higher tempering temperatures trade hardness for toughness and ductility.
| Condition | Tensile strength | Proof strength | Elongation | Typical use |
|---|---|---|---|---|
| Annealed | Order of 450 MPa | Order of 250 MPa | About 15% | Machining, forming, joints to be heat treated |
| Quenched and tempered | Substantially higher, set by tempering temperature | Substantially higher than annealed | Lower than annealed | Cutlery, valve parts, shafts, wear-resistant overlays |
Hardness rather than tensile strength is often the acceptance criterion for grade 420, precisely because the material is chosen for wear resistance. Hardness in the quenched and tempered condition is controlled by the tempering temperature, so the tempering schedule belongs on the drawing and should be checked against the consumable data sheet before production.
Equivalent Grades and Filler Metal Selection
The 420 type corresponds to the AISI 420 and EN 1.4021 martensitic stainless family, with chromium in the 12-14% range and carbon in the 0.25-0.40% range for consumables. Filler metal is selected to match the base metal composition and the mechanical properties required in service.
Match the chromium and carbon level of the base metal so that the weld metal hardens in the same way.
Keep preheat and interpass temperature within the qualified range to prevent cold cracking in the martensitic structure.
Schedule post-weld heat treatment while the joint is still warm where the qualified procedure allows it.
Check the guaranteed values against the manufacturer's data sheet and the governing standard edition.
Applications, Welding and Heat Treatment
Grade 420 is used for cutlery, turbine blades, valve parts and shafts, for repair welding of wear-resistant and corrosion-resistant 13% chromium components, and for hardfacing and overlay work where hardness after heat treatment is the objective.
Preheating, typically to 200-300 °C, together with controlled cooling, is recommended to avoid cracking of the martensitic weld metal. Post-weld heat treatment, either tempering or hardening and tempering, is normally required to restore toughness and to reach the target hardness. Where a component is to be used as-welded, the procedure should be qualified for that condition, because as-welded martensitic weld metal is hard and low in toughness.
Frequently Asked Questions
Q: What is 420 type welding consumable?
A: A martensitic stainless filler with 0.25-0.40% carbon and 12-14% chromium, covered by EN ISO 14343, used to weld 13% chromium martensitic steels such as AISI 420.
Q: Why is preheating required when welding grade 420?
A: Martensitic weld metal hardens as it cools and is prone to cracking. Preheating to 200-300 °C with controlled cooling reduces that risk and is followed by tempering or by hardening and tempering.
Q: What are the typical mechanical properties of grade 420?
A: Annealed weld metal in the 13% chromium family is on the order of 450 MPa tensile strength, 250 MPa proof strength and 15% elongation. Quenched and tempered material is substantially stronger and harder.
Q: What is grade 420 equivalent to?
A: The 420 type corresponds to the AISI 420 and EN 1.4021 martensitic stainless family.
Q: How is the hardness of grade 420 controlled?
A: Hardness is set mainly by the tempering temperature after quenching. Low tempering temperatures give the highest hardness, and higher tempering temperatures improve toughness.
Q: Can grade 420 be used as-welded?
A: It can, but as-welded martensitic weld metal is hard and low in toughness, so the welding procedure should be qualified for that condition and the service requirements checked.