Gnee Steel (tianjin) Co., Ltd
+8615824687445

S250GD Galvanized Steel:Surface Finish & Spangle Options

Jan 08, 2026

S250GD Galvanized Steel

 

S250GD is characterized by a balanced combination of strength, ductility and corrosion resistance. The minimum yield strength Rp0.2 of 250 N/mm² and a tensile strength in the range of 360-510 N/mm² guarantee a reliable load-bearing capacity with sufficient ductility. Thanks to the hot-dip galvanized surface, the steel achieves long-lasting corrosion protection, making it resistant even in aggressive climates and industrial environments.

 

Hot-dip galvanized steel S250GD in accordance with the EN 10346 standard is a high-quality structural steel that has been specially developed for use in the construction industry. With the material number 1.0242, S250GD has a minimum yield strength Rp0.2 of 250 N/mm² and is therefore classified in the medium strength classes of hot-dip galvanized structural steels. The EN 10346 standard not only specifies the chemical composition and mechanical properties, but also defines the hot-dip galvanizing process that creates a uniformly protective zinc coating on the steel surface. The available coatings +Z, +ZF, +ZA, +ZM, +AZ and +AS enable precise adaptation to different environmental conditions and load scenarios.

 

S250GD Galvanized Steel

 

Surface Finish & Spangle Options


GNEE STEEL provides a range of spangle finishes and surface treatments for S250GD galvanized steel, offering versatility for various applications.

 

Spangle Types:

Spangle refers to the crystalline structure that forms on the surface of galvanized steel. The spangle finish influences both the aesthetics and functional properties of the material:

 

Spangle Type Description
Normal Spangle Traditional, large crystalline spangle with visible metallic sheen.
Skinpassed Spangle A smooth, uniform spangle with reduced surface texture, offering a more polished appearance.
Minimized Spangle A subtle spangle with minimal crystalline formation, ideal for more refined aesthetics.
Regular Spangle Balanced spangle appearance with consistent texture, suitable for general use.

 

Surface Treatments:

In addition to spangle options, we offer various surface treatments to enhance the material's properties:

 

Surface Treatment Description
Chromate Passivation A corrosion-resistant chromate passivation layer for enhanced durability and weather resistance.
Oiled A light oil coating applied to prevent corrosion and maintain surface integrity during storage and handling.
Uncoated No additional surface coating, ideal for applications where a natural galvanized finish is desired.

 

DIN S250GD + Z DIN Mechanical properties

 

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
998 (≥) 825 (≥) 11 14 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

 

DIN S250GD + Z DIN Physical properties

 

The DIN S250GD + Z DIN  material physical properties shall comply with the values given in the following table.

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson's coefficient, ν
42 - -     0.14 -  
499 398 - 24.3 421   -  
341 - 11 21.2     434 221

 

Standard

Grade

C

Si

Mn

P

S

Ti

Forcold Forming

Chinese Standard

DX51D+Z

0.12

0.50

0.60

0.100

0.045

0.30

DX52D+Z

0.12

0.50

0.60

0.100

0.045

0.30

DX53D+Z

0.12

0.50

0.60

0.100

0.045

0.30

DX54D+Z

0.12

0.50

0.60

0.100

0.045

0.30

DX56D+Z

0.12

0.50

0.60

0.100

0.045

0.30

DX57D+Z

0.12

0.50

0.60

0.100

0.045

0.30

Forcold Forming

Japanese Standard

SGCC

0.15

0.50

0.80

0.050

0.030

0.025

SGCD1
SGCD2

0.12
0.10

0.50
0.50

0.60
0.45

0.040
0.030

0.030
0.030

0.025
0.025

SGCD3

0.08

0.50

0.45

0.030

0.030

0.025

SGCD4

0.06

0.50

0.45

0.030

0.030

0.025

For Structure

Japanese Standard

SGC340

0.25

0.50

1.70

0.200

0.035

0.025

SGC400
SGC440

0.25
0.25

0.50
0.50

1.70
2.00

0.200
0.200

0.035
0.035

0.150
0.150

SGC490

0.30

0.50

2.00

0.200

0.035

0.025

SGC510

0.30

0.50

2.50

0.200

0.035

0.025

For Structure

AISI Standard

S220GD+Z

0.20

0.60

0.70

0.100

0.045

0.025

S250GD+Z

0.20

0.60

0.70

0.100

0.045

0.025

S280GD+Z

0.20

0.60

0.70

0.100

0.045

0.025

S320GD+Z

0.20

0.60

0.70

0.100

0.045

0.025

S350GD+Z

0.20

0.60

0.70

0.100

0.045

0.150

S550GD+Z

0.20

0.60

0.70

0.100

0.045

0.150

 

Frequently Asked Questions (FAQ)

Q: What is S250GD steel?

A: S250GD steel is a galvanized steel known for its strength and durability. Due to its high yield strength and excellent corrosion resistance, it is commonly used in construction and manufacturing.

Q: What are the typical applications of S250GD galvanized coil?

A: S250GD galvanized coil is widely used in roofing, construction, automotive parts, and as a raw material for making galvanized steel plates, sheets, and pipes. Its resistance to corrosion makes it ideal for outdoor applications.

Q: How does the galvanizing process enhance the properties of S250GD steel?

A: The galvanizing process involves coating the steel with a zinc layer, providing a protective barrier against corrosion. This process enhances the durability and longevity of S250GD steel, making it suitable for various applications.

Q: What is the chemical composition of S250GD steel?

A: The chemical composition of S250GD steel typically includes carbon, manganese, phosphorus, sulfur, and a zinc coating. The specific composition balances strength, ductility, and corrosion resistance.

Q: What is the minimum yield strength of S250GD steel?

A: The minimum yield strength of S250GD steel is 250 MPa. This property ensures the steel can withstand significant stress and strain without deforming, making it a reliable choice for structural applications.

 