DC04 Vs SPCE Vs DC01 Vs DC05: Picking The Right Cold Rolled Grade

Oct 10, 2026

Cold Rolled Grade

 

DC04 sits in the middle of the cold forming ladder in EN 10130: softer and more drawable than DC03, stronger and cheaper than DC05. When buyers source it across borders they meet SPCE from Japan, DS or DDS from the United States, and DC04 again under GB/T 5213 from China. The names line up roughly, but "equivalent" is a sourcing shortcut, not a contract term. This page maps the grades and shows where the mapping breaks.

 

Cold Rolled Steel

 

1.Cross-Standard Map

EN 10130

JIS G 3141

ASTM A1008 / A1008M

GB/T 5213

Old DIN

DC01

SPCC

CS Type A / B

DC01

St 12-03

DC03

SPCD

DS Type A / B

DC03

St 13-03

DC04

SPCE

DDS

DC04

St 14-03

DC05

SPCF

-

DC05

St 15-03

DC06

SPCG

EDDS (IF)

DC06

-

Use this table to find a candidate, then confirm the actual limits in the standard you are buying to.

 

2.Where "Equivalent" Breaks Down

Four differences cause real problems when a grade is substituted across systems.

 

Elongation is measured on different gauge lengths.

EN 10130 uses A80, an 80 mm gauge length. ASTM A1008 uses 50 mm (2 in). A shorter gauge length reports a higher percentage for the same material, so an A50 figure is not comparable with an A80 figure and must never be pasted into an EN datasheet.

Chemistry windows differ.

DC04 limits carbon to 0.08 % and manganese to 0.40 %. The JIS and ASTM grades in the same row allow different ceilings, which changes weld behaviour and coating response in ways the row does not show.

Surface designation is not shared.

EN 10130 uses quality classes A and B with finishes b, g, m and r by roughness. JIS uses its own bright and dull designations for SPCC. A purchase order that says "equivalent to DC04" says nothing about surface.

Non-ageing is a separate requirement.

Standard DC04 is not guaranteed non-ageing. Where parts are stored before forming, or where stretcher strains cannot be tolerated on a visible panel, the Japanese system offers SPCEN and the EN system moves to DC05 or DC06. Ask for it by name.

 

3.When to Step Down or Step Up

Grade selection should follow the part, not the price list. Over-specifying DC05 on a bracket wastes money; under-specifying DC01 on a deep cup produces scrap.

 

Part or process

Recommended grade

Simple blanking, bending, embossing

DC01

Moderate drawing, shallow profiles

DC03

Deep drawing, complex single-hit forms

DC04

Severe or extreme draws

DC05 / DC06

Visible panels stored before forming

Non-ageing grade, DC05 or above

Parts where the drawing indicators are critical

DC04 with r90 and n90 agreed at order

Anything with a calculated load

Not a DC grade - use a structural grade with a minimum yield

That last row matters. DC04 has no minimum yield strength to design against. If a bracket carries a load that has to be calculated, the DC ladder is the wrong family, however well it forms.

 

4.Buying Notes

 

Tolerance class changes price.

EN 10131 normal class for 0.80–1.00 mm is ±0.05 mm; the special class is roughly 20–30 % tighter. Confirm which one is quoted.

Ask for r90 and n90 at enquiry, not at delivery.

They are only reported when agreed in the order.

Order surface explicitly.

Class A or B, finish b, g, m or r.

Trial before volume.

Sample coils let you run your own tooling before committing, and they settle arguments about formability faster than any datasheet.

 

FAQ

Q: Is SPCE the same as DC04?

A: SPCE is the usual Japanese equivalent for sourcing, but the chemistry windows, surface designation and test basis differ. Confirm limits before substituting.

Q: Why is the A1008 elongation figure higher than EN 10130's?

A: A1008 measures elongation on a 50 mm gauge length and EN 10130 on 80 mm. Shorter gauge lengths report higher percentages for the same steel, so the numbers are not comparable.

Q: Can I use DC04 for a load-bearing bracket?

A: Not for a calculated load. DC04 has no guaranteed minimum yield strength.

Q: When should I move from DC04 to DC05?

A: When the draw depth exceeds what DC04 forms without necking, or when the part must not age between delivery and forming.

 

We supply the full EN 10130 range and can quote DC01 through DC06 against one drawing so you can compare before committing. Send the part geometry and we will recommend the grade that clears the draw at the lowest cost.