Ferritic stainless steel cannot be strengthened by heat treatment because it has no phase transformation. Generally, it is used after annealing at 700~800℃. Since the atomic siz...

May 26, 2022
(1) Uniform corrosion. Chromium is the easiest element to passivate. In the atmospheric environment, iron-chromium alloys with a chromium content of more than 12% can be self-pa...

May 26, 2022
According to the purity of the steel, especially the content of carbon and nitrogen impurities, it can be divided into ordinary ferritic stainless steel and ultra-pure ferritic ...

May 26, 2022
Generally, it can be divided into two categories: ordinary ferritic stainless steel and high-purity ferritic stainless steel.

May 26, 2022
What is the Ferritic Stainless Steel? Ferritic stainless steel (400 series) has a chromium content of 15% to 30% and has a body-centered cubic crystal structure. This type of st...

May 26, 2022
Ordinary ferritic stainless steel is sensitive to notches, and the brittle transition temperature is above room temperature except for low chromium (such as 405). The higher the...

May 26, 2022
Corrosion resistance can be modified depending on the service environment.

May 26, 2022
For example, the uses include making minuscule parts for wristwatches. At the same time, large panels with a certain surface finish may cover whole buildings.